Russell Wanhill & Michael Windisch 
Corrosion and Stress Corrosion Testing of Aerospace Vehicle Structural Alloys [PDF ebook] 

สนับสนุน

This Springer Brief discusses the determination and classification of the ambient temperature corrosion and stress corrosion properties of aerospace structural alloys, with emphasis on (1) aluminium alloys, modern (3rd generation) aluminium‒lithium alloys, stainless steels and titanium alloys and (2) some of the issues involved. Standard /reference data on environmental properties, including corrosion and stress corrosion, are mandatory for the qualification and certification of materials for aerospace vehicles, and also for the design of actual structures and components. Recommendations for further testing and evaluation are given at appropriate points in the text. The book concludes with a summary of the main topics.  

€58.84
วิธีการชำระเงิน

สารบัญ

1. Introduction.- 2. Corrosion.- 3. Stress Corrosion Cracking (SCC).- 4. Environmental severities: natural/outdoor versus accelerated testing.- 5. Aluminium-lithium alloys: some corrosion and SCC issues.- 6. Stainless steels: some corrosion and SCC issues.- 7. Titanium alloys: special issues and aspects concerned with SCC testing.- 8. Summary.- Acknowledgements.- References.

ซื้อ eBook เล่มนี้และรับฟรีอีก 1 เล่ม!
ภาษา อังกฤษ ● รูป PDF ● หน้า 63 ● ISBN 9783319895307 ● ขนาดไฟล์ 3.3 MB ● สำนักพิมพ์ Springer International Publishing ● เมือง Cham ● ประเทศ CH ● การตีพิมพ์ 2018 ● ที่สามารถดาวน์โหลดได้ 24 เดือน ● เงินตรา EUR ● ID 6281838 ● ป้องกันการคัดลอก โซเชียล DRM

หนังสืออิเล็กทรอนิกส์เพิ่มเติมจากผู้แต่งคนเดียวกัน / บรรณาธิการ

699 หนังสืออิเล็กทรอนิกส์ในหมวดหมู่นี้